Frost Salt Scaling Resistance Improvement of GGBFS Concrete by Na-MFP Treatment
DOI:
https://doi.org/10.33593/iccp.v8i1.569Keywords:
GGBFS, Na-MFP, frost salt scaling, treatment, carbonate phasesAbstract
An investigation has been performed into a treatment of the surface of ground granulated blast furnace slag (GGBFS) cement concrete in order to improve the frost salt scaling resistance. A sodium monofluorophosphate (Na- MFP) solution has been applied. The results show that the resistance is substantially improved. The microstructural characteristics are also discussed. In addition, the effect of various percentages of Na-MFP solution on frost salt scaling resistance of GGBFS mortar phase is presented. It is concluded that the Na-MFP treatment modifies the carbonate phases and improves the early resistance of the GGBFS cement matrix with water to cement ratio of 0.45 against frost salt scaling attack.
Downloads
Published
2025-01-17
Issue
Section
Articles
How to Cite
[1]
Çopuroglu, O. et al. 2025. Frost Salt Scaling Resistance Improvement of GGBFS Concrete by Na-MFP Treatment. Proceedings of the International Conference on Concrete Pavements. 8, 1 (Jan. 2025). DOI:https://doi.org/10.33593/iccp.v8i1.569.