PERFORMANCE OF ULTRA-THIN WHITETOPPING IN FLORIDA
DOI:
https://doi.org/10.33593/iccp.v6i1.705Keywords:
concrete, ultra-thin whitetopping, design, rehabilitation, fibers, high early strength, falling weight deflectometer, FWDAbstract
Three experimental test tracks were constructed in Gainesville, Florida to evaluate design, construction and performance of the ultra-thin whitetopping (UTW). In Test Track 1, a 100-mm (4-in.) thick UTW was placed on existing pavement composed of 38-mm (1.5-in.) asphalt pavement and 150-mm (6-in.) concrete base. The surface of the asphalt pavement was prepared in three ways: milling, broom cleaning, and applying a thin asphalt crack relief layer (CRL). Test Track 2 consisted of 75-mm (3-in.) and 100-mm (4-in.) thick sections on a 38-mm (1.5-in.) asphalt pavement and a 163-mm (6.5-in.) base layer of sand and Florida limerock material. The surface of the asphalt pavement was prepared in two ways: milling and broom cleaning. In Test Track 3, a 50-mm (2-in.) thick concrete overlay was placed on 38-mm (1.5-in.) milled asphalt pavement and 163-mm (6.5-in.) base layer similar .to that in Test Track 2. Joint spacings in Tracks 1 and 2 were 1.22 m X 1.22 m (4 ft X 4 ft) and 1.83 m X 1.83 m (6 ft X 6 ft). Test Track 3 had 0.92 m X 0.92 m (3 ft X 3 ft) and 1.22 m X 1.22 m (4 ft X 4 ft) joint spacings. Polypropylene fibers were used in Tracks 1 and 2. Polyolefin fibers were used in Track 3. High early strength concrete was designed for the UTW. Bond strength at the concrete-asphalt interface was generally above 1.4 MPa (200 psi). The test tracks were subjected to approximately 60,000 (18-kip) ESALs using a truck loaded with concrete blocks. Falling Weight Deflectometer (FWD) test results showed significant improvement in the structural capacity of the pavement after placement of the UTW. Frequent condition surveys indicated excellent performance of the three test tracks. The UTW is a viable option for rehabilitation and restoration of asphalt pavements.